CuproShield IC semiconductor copper anti-tarnish agent is a water-soluble protective agent for copper. It prevents oxidation on the surfaces of electroless copper, electroplated copper, as well as other copper and copper alloys. The protective film formed is colorless and transparent, significantly improving the corrosion resistance of copper surfaces after application. Free of chromates, it does not pollute the environment and is highly economical to use.
CuproShield IC semiconductor copper anti-tarnish agent can also be applied in the final water-rinse stage after copper plating, keeping the copper surface fresh and pink while preventing oxidation. Copper surfaces treated with CuproShield IC semiconductor copper anti-tarnish agent do not require subsequent water rinsing. The protective film formed by CuproShield IC semiconductor copper anti-tarnish agent is easily removed with acidic or alkaline degreasers; under normal conditions, the film can be completely stripped by degreasing followed by acid washing, allowing immediate subsequent electroplating operations.
1. Operating Conditions
| Operating Parameter | Unit | Conditions |
|---|---|---|
| CuproShield IC semiconductor copper anti‑tarnish agent | % | 5‑20 |
| CuproShield IC semiconductor copper anti‑tarnish agent (Low Concentration) | % | 5 |
| Temperature | °C | 25‑50 |
| Immersion Time | sec | Minimum 20–60 |
2. Operating Instructions
Workpiece immersion in the CuproShield IC semiconductor copper anti-tarnish agent solution is the final step prior to drying. After treatment with CuproShield IC semiconductor copper anti-tarnish agent, two stages of deionized (DI) water rinsing are required; standard water rinsing can also be omitted, depending primarily on cosmetic requirements, without affecting the formed protective film. To accelerate drying, the CuproShield IC semiconductor copper anti-tarnish agent solution can also be operated at an elevated temperature of 50°C.
Workpieces must be clean, wet, and free of oil/grease before entering the CuproShield IC semiconductor copper anti-tarnish agent bath. Because CuproShield IC semiconductor copper anti-tarnish agent has no cleaning action, a protective film will not form on contaminated surfaces. If the process prior to entering CuproShield IC semiconductor copper anti-tarnish agent is acidic, care must be taken during production to prevent drag-in of excess acid solution, which could compromise the treatment efficacy of CuproShield IC semiconductor copper anti-tarnish agent.
3. Equipment
The CuproShield IC semiconductor copper anti-tarnish agent solution must be stored in stainless steel, fiberglass, plastic, PVC-lined steel, PE (polyethylene), or PP (polypropylene) tanks. Using plain carbon steel tanks will cause rusting and adversely affect the formation of the CuproShield IC semiconductor copper anti-tarnish agent protective film. Heaters may be made of quartz, stainless steel, or Teflon (PTFE). It is recommended to equip the production line with an exhaust ventilation system.
4. Control and Maintenance
Normally, the CuproShield IC semiconductor copper anti-tarnish agent solution does not require replacement based on a fixed surface area processed per liter. Susceptibility of workpieces to oxidation indicates that the active components in the solution are low or contaminated, requiring bath replacement. Analytical methods can be provided upon request.
5. Waste Treatment
Wastewater discharge must comply with local regulatory standards.
6. Disclaimer
All suggestions or recommendations regarding our products contained in this technical data sheet are based on experiments and data believed to be reliable by our company. Since actual operations by third parties are beyond our control, our company guarantees no performance outcomes and accepts no liability for any adverse results. Nothing in this document shall be construed as evidence of or authorization for patent or copyright infringement.